What did TANIOBIS demonstrate on the four-laser machine?
Parameters first developed on a single-laser AM400 moved to a four-laser AM500Q with only minor adjustments. Parts showed porosity under 0.1% and density above 99.9%. To test consistency, the team spread 52 cubes randomly over the plate using the four best parameter sets, and porosity stayed below 0.3% everywhere, apart from a few outliers likely caused by spatter.
Nozzles of 53 mm diameter and 100 mm height followed, without visible defects. Early builds used one laser to prove reproducibility, later ones used all four at once to raise throughput. The C-103 process window widened on the AM500Q to 95 to 255 J/mm³.
How do the two alloys compare in strength and heat?
FS-85 is the stronger grade at room temperature, about 750 MPa tensile strength against 565 MPa for C-103, and it is stiffer. C-103 is the more ductile one, stretching 20 to 22% before fracture against 6 to 7% for FS-85. Heat treatment can raise elongation of both to about 30% with little strength loss.
At high temperature FS-85 led across the tested range up to 1,600 °C: at 1,500 °C it still carried roughly 220 MPa tensile strength while C-103 had almost none left. Printed C-103 was clearly stronger than rolled C-103 (557 against 420 MPa tensile), though the gap narrowed above about 800 °C. As-built grains are elongated along the build axis, so properties depend on direction.
Powder, parameters and the wider qualification effort
The powder came from EIGA atomization, sieved to 15 to 63 µm, with near-spherical particles. On the AM400, C-103 tolerated 160 to 240 J/mm³ while FS-85 needed a narrower 105 to 125 J/mm³. Tuning cut porosity from about 1% to 0.06%.
TANIOBIS has signed Elmet Technologies to distribute both powders in North America. Elsewhere, Elmet installed a 3D Systems DMP Flex 350 Triple with tight oxygen control, Velo3D is qualifying Amaero's C103 powder, and America Makes and NCDMM awarded $6 million for refractory alloy work. C103 powder can cost up to $4,000 per kg.